Hairline cracks in top plate

Hairline cracks on top plate at join point of screws (present on all machines inspected so far). The top plate uses a 3-layer design, and the cracks affect only the top plate. The fluid path is accessed via the arm port and not affected by the presence of these cracks, so this defect is cosmetic. Cracks are most noticeable under direct light, some are barely visible.

 

B Grade — $549

  • Hairline cracks on top screws
  • Possibility of 1-3 small scratches/light scuffing on chassis; may be more noticeable in direct bright light
  • Possibility of light scuffing on portions of dustcover
  • Please note: any visible "specks" are dust

 

C Grade — $515

  • Hairline cracks on top screws
  • Scratches/scuffing on chassis that are likely to be larger or more pronounced; may be noticeable in a wider variety of lighting
  • Possibility of heavy scuffing on portions of dustcover
  • Please note: any visible "specks" are dust